Material: 35Mn2Si
Technology: Casting
Heat treatment: full hardening and tempering, surface hardening.
Warranty: 2000-2500 working hours
Place of Origin: Shandong, China(Mainland)
Supply Ability: 5000 pcs/ Month
Warranty: 2000-2500 Working Hours
Min Order Quantity: 1 Piece
Package Detail: Export Standard Pallet/ Plywood Case
Port of Loading: Yantai, Qingdao, Shanghai
Trade Terms: EXW, FOB, CFR, CIF
All casting should be Austenitized at 900°C for one Hr per every inch of casting thickness.
Then Quenched on water and Tempered for sufficient amount of temperature and time.
All heat treatment should be carried out after castings reach temperature lower than 200°C.
The general hardness after QT to be 230-320 BHN.
Link belt LS138HII track shoe have high bending strength and wear resistance.
Link belt LS138HII track pad 's pitch must be accurately adjusted to avoid pinching stones between two adjacent Link belt LS138HII track shoe.
Link belt LS138HII track plate must be installed in the same direction to form the belt of the head and tail.
In this way, the work uniformity is good, the wear of the Link belt LS138HII track shoe is low, and the running efficiency is high during work.